MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Omnia Plastica PVC Polyvinylchloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Extruded

Material Notes: A widely used material, its application is under regulation in many countries for ecological reasons and it is often substituted by PP or other polymers. It is chosen for its chemical resistance.

Features:

  • High chemical resistance
  • Higher stiffness compared to polyolefins
  • Easy machinability on mechanical tools. It can be hot welded
  • Colour: grey, ivory, red
Weak Point:

Compared to PP it has lower shock and temperature resistance. The high gravity reduces its cheapness.

Application:

  • Chemical: the main application of PVC is in the chemical industry, thanks to its high resistance to acids and alkali and to its rigidity. It is used for components such as valves, flanges, gears, etc. in the chemical, galvanic and petrochemical industries.
  • Food contact: it cannot be used in contact with food.
  • Electrical: good dielectric properties and weather resistance make it suitable for these applications.
  • Mechanical: it is also used for mechanical components in corrosive environments. Compared to polyolefins, it has a higher tensile stress.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors:
Available Properties
  • Density, ISO.1183 DIN.53479
  • Moisture Absorption at Equilibrium, 50% relative humidity
  • Water Absorption at Saturation, 23°C
  • Hardness, Rockwell M, ISO2039.2, dry sample
  • Ball Indentation Hardness, ISO2039.1 DIN.53456
  • Tensile Strength at Break, ISO.527 DIN.53455
  • Elongation at Break, ISO.527 DIN.53455
  • Tensile Modulus, ISO.527 DIN.53455
  • Compressive Strength, ISO.899 DIN.53444, 1% strain over 1000 hours
  • Charpy Impact Unnotched, ISO.R179 DIN.53453, 7.5 J
  • Charpy Impact, Notched, ISO179/3C DIN.53453
  • Volume Resistivity, ISO.93 DIN.53482
  • Dielectric Constant, ISO.250 DIN.53483
  • Dielectric Strength, ISO.243 DIN.53481
  • Dissipation Factor, ISO.250 DIN.53483
  • CTE, linear
  • Thermal Conductivity, DIN.52612
  • Melting Point
  • Maximum Service Temperature, Air, Continuous; 5000 hours based on a tensile stress of 50% at 23° C.
  • Maximum Service Temperature, Air, short period, no load
  • Deflection Temperature at 1.8 MPa (264 psi), ISO.75 DIN.53461
  • Minimum Service Temperature, Air, impact conditions and heavy loads not considered
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Omnia Plastica s.p.a.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.