MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger SPI
Ensinger TECASON™ S Polysulfone (PSU)
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: TECASON™ S is a transparent engineering plastic known for its chemical resistance, rigidity, high-temperature performance, and its ability to operate in an autoclave environment. TECASON™ S is FDA and NSF compliant and holds its excellent mechanical properties over a wide range of temperatures.

  • Autoclave resistance (maintains dimensional stability and mechanical performance through repeated autoclaves)
  • Excellent electrical properties
  • Good chemical resistance (performs well in mineral acids, alkali, salt solutions, and hydrocarbons)
  • Superior resistance to creep
  • FDA and NSF compliant
  • High-temperature performance (has a heat deflection temperature of 345°F and a long-term continuous use temperature of 285°F)
  • Excellent hydrolytic stability
  • High strength and rigidity
  • Flame retardant (rated UL94 V-O)

TECASON™ S' unique combination of chemical and hydrolytic resistance, high-temperature performance, good mechanical properties, and agency approvals make it an excellent choice for applications in pharmaceutical, medical, food service equipment, semiconductor processing, and electronic equipment industries.

Information Provided by Ensinger Industries, Inc.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength at Break, ASTM D638
  • Elongation at Break, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Coefficient of Friction, Dynamic, 50 fpm
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150, 50% RH
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM D696
  • Maximum Service Temperature, Air, Long Term
  • Maximum Service Temperature, Air, Short Term
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point
  • Transmission, Visible, transparent; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.