| Structure of material: Open cell Polyurethane foam-self-extinguishing and impregnated type Class 1; Open cell-elastic melamine resin Class 1; Thermobonded Polyester fiber; Coupled with lead sheet and elastomer mass Application: Materials above mentioned can be used as sound-absorbers into the air canalizations, into the structure of noisy machineries and tools and they can be cut in shaped pieces and sizes on request. For example: compressor casing, noiseless cabinets, gymnastic rooms, recording studios, false ceilings, tooling machines, partition walls Aspect: Coupled with PU, ALU and PVC film; Smooth; Embossed; Pyramidal shaped Information provided by Eurofoam s.r.l. |