MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Master Bond EP17HT-LO One component epoxy system for bonding, sealing, coating and casting
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Description: Master Bond EP17HT-LO is a one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation profile and chemical resistance even with heat exposure to 650°F. Its glass transition temperature (Tg) is 225°C. This system is also has very low exotherm upon curing and can be used in castings and encapsulations well beyond ½ inch in thickness. The minimum curing temperature for EP17HT-LO is 300°F with faster cures attainable at higher temperatures. EP17HT-LO is 100% reactive and contains no solvents or diluents. EP17HT-LO bonds well to similar as well as dissimilar substrates such as metal, ceramics, plastics and composites. It has resistance to many chemicals such as acids, bases, salts, fuels, oils and many solvents. Shrinkage upon cure is minimal. It is serviceable from -80°F to +650°F. This system is tan in color. EP17HT-LO retains its electrical insulation properties, even at higher temperatures. It should be noted, in order to obtain the optimum properties, a post cure of 2-12 hours at 350°F is recommended. As mentioned above, EP17HT-LO meets NASA low outgassing specifications. It is widely used in a variety of applications in the aerospace, oil and chemical processing, optical, opto-electronic and specialty OEM industries.

Product Advantages:

  • Single component system; no mixing prior to use. Contains no solvents, diluents or volatiles
  • Easy application; only positive contact pressure required during heat cure
  • Good tensile, shear and compressive strength properties
  • Certified to NASA low outgassing standards
  • High temperature resistance. Staggering Tg

Information provided by MasterBond®

Vendors:
Available Properties
  • Solids Content
  • Viscosity
  • Hardness, Shore D
  • Tensile Strength at Break
  • Tensile Modulus
  • Compressive Strength
  • Shear Strength
  • Shear Strength, tensile lap, aluminum to aluminum
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dissipation Factor
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time
  • Cure Time
  • Cure Time, plus 2-12 hrs at 350°F
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.