Product overview: This product is prepared by catalytic cracking under the action of Ni / Al2O3 catalyst. Hydroxylated and carboxylated derivatives are available. (Prepared by KMnO4 oxidation in H2SO4 solutions under different temperatures and concentrations.) Application: This material can be used in polymer additives, catalysts, flat panel display, nanotube composites (by filling or coating), etc. Information provided by Matexcel |