MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
NOVA Chemicals SURPASS® RMs245-UG sHDPE Rotational Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Rotational Molding Grade

Material Notes:

Octene Copolymer

Features:

  • Exceptional low temperature impact properties
  • Broad processing window
  • High stiffness for very large tanks, combined with exceptional ESCR performance
  • Superior whiteness for improved part appearance, resistant to gas fading
  • NSF listed for Standards #24, 51, 61
  • Broad application use and potential for resin consolidation
  • Good interior finish on large tanks
  • UL94 HB
  • HDB rating 1600 psi

Additives:

  • Processing antioxidants
  • UV stabilizers (estimated UV resistance > UV20)

Applications:

  • Septic tanks
  • Very large tanks (up to 20,000 gallons)
  • Agricultural tanks as small as 3,000 gallons

United States: SURPASS RMs245-U(UG) resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may contact food only at temperatures of 212°F and below (21 CFR 176.170(c) Table 2, conditions of use B–H).

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors:
Available Properties
  • Density, ASTM D 792
  • ESCR 100% Igepal®, ASTM D 1693, F50, Condition A & B
  • Melt Index of Compound, ASTM D 1238
  • Tensile Strength, Yield, ASTM D 638, Type IV specimen, 2" (50.8 mm) per minute test speed
  • Elongation at Yield, ASTM D 638, Type IV Specimen, 2" (50.8 mm) per minute test speed
  • Flexural Modulus, ASTM D 790
  • Impact Test, ARM Method, ARM Low Temperature Impact
  • Impact Test, ARM Method, ARM Low Temperature Impact
  • Melting Point, (DSC)
  • Heat Distortion Temperature, ASTM D 648
  • Heat Distortion Temperature, ASTM D 648
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.