| Catalyst Masterbatch CT/2-LR is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for CogegumĀ® GFR series compounds, it allows easy processing during extrusion. It has the same features of CT/2, but with a lower catalytic activity. Catalyst Masterbatch CT/2-LR can be used in a wide application range due to its catalytic activity and the anti-ageing effect given to the final product. It contains also a metal deactivator that allows its use also in direct contact with untinned copper Copper Contact Stabilized; Halogen Free Uses: Wire & Cable Applications Availability: Asia Pacific; Europe; North America Information provided by Solvay Specialty Polymers. |