MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Microtherm Group Aeroguard® HD Filament Reinforced Silica Thermal Insulation Panel, Flexible
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Aeroguard® is a Microtherm® Flexible Insulation Panel made under the most stringent quality control with full traceability for aerospace applications.
    Properties
  • Opacified blend of filament reinforced silica
  • Flexible Aerospace quality high temperature microporous insulation
  • Lowest thermal conductivity
  • Stable performance for continuous exposure to 1000 °C (1832 °F)
  • Non combustible. Aeroguard® HD can withstand direct fire exposure without damage
  • Easy to manipulate and shape
  • Environmentally friendly.
    Applications
  • Aircraft
  • Missiles
  • Intelligent armaments

Information provided by Microtherm.

Vendors:
Available Properties
  • Density, dependent on panel grade, area and thickness
  • Thickness
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity, @ 200 kg/m³
  • Thermal Conductivity, @ 200 kg/m³
  • Thermal Conductivity, @ 200 kg/m³
  • Thermal Conductivity, @ 200 kg/m³
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.