MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Braskem INSPIRE™ 114 Performance Polypropylene Polymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Blow Molding Grade; Polypropylene, Extrusion Grade; Polypropylene, Impact Modified; Molded/Extruded; Polypropylene, Sheet/Thermoforming Grade

Material Notes:
    Overview
  • High melt strength
  • High toughness
  • Excellent processability
  • High impact and puncture resistance
  • High film stiffness/machinability
  • High heat resistance
  • Complies with U.S. FDA FCN 843, Europe EU-Directive 2002/72/EC

INSPIRE™ 144 Performance Polymer is intended for use in blown film extrusion. Film produced from this resin offers improved stiffness, heat resistance, creep resistance, puncture strength and toughness over competitive polyethylene films. Coextruded structures offer a broad range of potential properties including high stiffness, high clarity, excellent sealability and good barrier properties. INSPIRE 114 Performance Polymer offers high output rates, thin or thick film production with excellent bubble stability, and good gauge uniformity.

INSPIRE™ 114 Performance Polymer is a propylene-based resin that is also intended for use in sheet extrusion, thermoforming, and blow molding.

This product line was spun off from Dow Chemical to Braskem

Vendors:
Available Properties
  • Density, ASTM D792
  • Thickness, Film Thickness
  • Melt Index of Compound, ASTM D1238
  • Film Tensile Strength at Yield, MD, ASTM D882, 50.8 microns, Blown Film
  • Film Tensile Strength at Yield, TD, ASTM D882, 50.8 microns, Blown Film
  • Tensile Strength, Yield, ASTM D638
  • Film Elongation at Break, MD, ASTM D882, 50.8 microns, Blown Film
  • Film Elongation at Break, TD, ASTM D882, 50.8 microns, Blown Film
  • Film Elongation at Yield, MD, ASTM D882, 50.8 microns, Blown Film
  • Film Elongation at Yield, TD, ASTM D882, 50.8 microns, Blown Film
  • Elongation at Yield, ASTM D638
  • Flexural Modulus, 1% Secant, ASTM D790A
  • Secant Modulus, MD, ASTM D882, 2% secant modulus
  • Secant Modulus, TD, ASTM D882, 2% secant modulus
  • Izod Impact, Notched, ASTM D256A
  • Dart Drop Test, ASTM D1709A, 50.8 microns, Blown Film
  • Film Tensile Strength at Break, MD, ASTM D882, 50.8 microns, Blown Film
  • Film Tensile Strength at Break, TD, ASTM D882, 50.8 microns, Blown Film
  • Melting Point, Dow Method, DSC
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.