| Formlabs IBT Flex Resin is a biocompatible compound with exceptional flexibility, strength, translucency, and colour, ensuring superior clinical results and optimal patient satisfaction. This versatile material allows for the efficient and accurate placement of orthodontic brackets and restorative composites, allowing you to create translucent trays and guides that are both pliable and durable, resulting in consistent and reliable outcomes. Applications - Indirect Bonding Trays
- Direct composite restoration guides
Benefits & Features - Class I Biocompatible material, FDA Registered
- Enhanced elongation and flexibility | Seamless intraoral placement and removal that provides fast and accurate bracket placement and perfect seating of guides on the dentition
- High Print Accuracy and Predictable Results | This material optimizes viscoelasticity to ensure accurate transfer of a digital set-up to the clinical scenario. It reduces the need for additional adjustments intraorally.
- Optimized Translucency and Color | This new formulation allows for easy visualization of critical elements such as brackets, restorative composite materials, and teeth.
Information provided by Proto3000
|