ANTI-AIR™ is an additive for HAPCO’S polymer alloy products, which aids in the release of bubbles caused by entrapped air. ANTI-AIR™ is added during the mixing process or can be pre-dispersed in the ‘B’ side, before proportioning the components. ANTI-AIR™ reduces surface tension, which will aid in faster vacuum degassing. Mix Ratio Methods: Starting point is .0004 parts per 100 parts of ‘B’. Add up to .0016 to the ‘B’ side by weight, mix well. Information provided by Hapco, Inc. |