Dimension Range: Cold rolled / GI, GA, ZA: thickness 0.80-2.00 mm, width up to 1500 mm. Hot rolled / UC: thickness 2.00-6.00 mm, width up to 1600 mm. Hot rolled / GI: thickness 2.00-2.50 mm, width up to 1120 mm. Slit strip and cut to length sheets are available upon request. Grade and coating specific restrictions on available dimensions may occur.
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category Notesnone