MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Reltek BONDiT™ B-45 Adhesive, Sealant & Coating System
Categories: Polymer; Adhesive; Thermoset

Material Notes: Key Properties:
  • Excellent adhesive for low surface energy plastics without primer.
  • Used in potting, painting and protective coating applications.
  • Excellent thermal and mechanical shock resistance.
  • Ease of use.

Applications: Flexible to 130% elongation, good chemical resistance. Bonds to most plastics, rubber, polyurethane, metals, ceramic and concrete. Tough, flexible, chemically resistant, non-blush clear coating with medium gloss finish. Potting compound alternative to castable polyurethanes, particularly for electrical cable/connector/transducer termination. Excellent for electrical and electronic applications as protective encapsulate against very wide range of environmental exposures, particularly moisture and sea water. Can be applied to oily surfaces. Will cure underwater. Ambient cure 24 hours or 3 hours at 100°C for full cure.

Key Words: Epoxy Adhesive, Sealant
Vendors:
Available Properties
  • Oil Absorption, 60 days ambient, Isopar M
  • Water Absorption, 90 days ambient DI water
  • Viscosity
  • Tensile Strength at Break, Post Cure 180°F, 24h
  • Tensile Strength, Ultimate, Peak; Post Cure 180°F, 24h
  • Tensile Strength, Yield, Post Cure 180°F, 24h
  • Elongation at Break, Post Cure 180°F, 24h
  • Elongation at Yield, Post Cure 180°F, 24h
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Ambient Set
  • Cure Time, Ambient, 97% cure
  • Cure Time, 98% cure
  • Tack-Free Time, Ambient
  • Pot Life, Ambient
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Reltek LLC

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.