MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Tra-Con Tra-Bond 724-14C Polyurethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: TRA-BOND 724-14C premixed and frozen, polyurethane adhesive is designed for good adhesion, providing strong, resilient bonds to a wide variety of substrates, including aluminum, solder, nylon, mylar and steel. Adhesive strength is maintained even in cryogenic conditions. This resilient adhesive can also be used for tacking wires and as a protective coating. TRA-BOND 724-14C adhesive exhibits good dielectric properties. There are several cure options, including curing at room temperature. It contains a fluorescent trace for inspection purposes.

Information provided by Tra-Con Inc.

Vendors:
Available Properties
  • Specific Gravity, Mixed
  • Viscosity, Mixed
  • Hardness, Shore A
  • Adhesive Bond Strength, Lap shear, alum to alum
  • Peel Strength
  • Volume Resistivity
  • Dielectric Constant
  • Extrusion Rate, 15 gauge needle @ 80 psi
  • Cure Time
  • Cure Time
  • Cure Time
  • Working Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Tra-Con, Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.