MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Domo TECHNYL® A 216 Black 21 N PA 66, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Description: TECHNYL ® A 216 Black 21 N is an unreinforced polyamide 66, standard viscosity, for injection molding. It is available in black color.

Key Properties: Chemical resistance; Good thermal properties

Benefits: This product offers all of the primary properties of unreinforced polyamide 66 : thermal and mechanical properties, chemical resistance, impact and abrasion resistance.

Applications: It is used in a wide variety of industries.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors:
Available Properties
  • Density, ISO 1183/A
  • Water Absorption, ISO 62
  • Linear Mold Shrinkage, Isotropy
  • Linear Mold Shrinkage, Flow
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength at Break, ISO 527 Type 1A
  • Tensile Strength, Yield, ISO 527 Type 1A
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Tensile Stress at Strain
  • Elongation at Break, ASTM D638
  • Elongation at Break, ISO 527 Type 1A
  • Elongation at Yield, ISO 527 Type 1A
  • Tensile Modulus, ISO 527 Type 1A
  • Flexural Strength, ISO 178
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ISO 178
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180/1A
  • Izod Impact, Unnotched (ISO), ISO 180/1U
  • Charpy Impact Unnotched, ISO 179/1eU
  • Charpy Impact, Notched, ISO 179/1eA
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112, Sol B
  • Comparative Tracking Index, IEC 60112, Sol A
  • CTE, linear, Transverse to Flow, ASTM D696
  • Melting Point, ISO 11357
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75/Bf
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75/Af
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94, ISO 1210
  • Flammability, UL94, ISO 1210
  • Oxygen Index, ISO 4589
  • Glow Wire Test, ISO 60695-2-12, Flammability Index
  • Glow Wire Test, ISO 60695-2-13, Ignition Temp
  • Processing Temperature, Compression zone
  • Processing Temperature, Mixing zone
  • Feed Temperature
  • Drying Temperature
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.