MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Bohler-Uddeholm UDDEHOLM ALVAR 14 Hot Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: Alvar 14 is a chromium-nickel-molybdenumvanadium alloyed steel

ALVAR 14 is characterized by:

  • Good toughness
  • Good resistance to high thermal stresses
  • Good stability in hardening
  • Good through-hardening properties

Applications:

    Alvar 14 is ideally suited for hot working tools such as:
  • Support parts for extrusion tooling, e.g. backers, bolsters
  • Hot forging tools
  • Die for tin, lead and zinc alloys
  • Tools for hot shearing

Key Words: W.Nr. 1.2714; NiCrMoV7
Vendors:
Available Properties
  • Density, hardness of 40 HRC
  • Density, hardness of 40 HRC
  • Density, hardness of 40 HRC
  • Hardness, Brinell, Soft annealed
  • Hardness, Brinell, Hardened and tempered (36-43 HRC, 1100-1350 Nmm2)
  • Modulus of Elasticity, (hardness of 40 HRC)
  • Modulus of Elasticity, hardness of 40 HRC
  • Modulus of Elasticity, hardness of 40 HRC
  • CTE, linear, hardness of 40 HRC
  • CTE, linear, hardness of 40 HRC
  • Thermal Conductivity, hardness of 40 HRC
  • Thermal Conductivity, hardness of 40 HRC
  • Thermal Conductivity, hardness of 40 HRC
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  • Vanadium, V
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.