MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Chemical Concepts Chem-Set™ 1201 RED INSULATING VARNISH
Categories: Polymer; Adhesive; Thermoset

Material Notes: Glyptal® 1201 Red Enamel Insulator was originally developed as an insulating paint for electrical applications such as the treatment of coils and armatures. Its outstanding resistance to corrosion, moisture, oil, acid, heat, dust and salt spray has made it popular throughout industry as a primer, sealer, adhesive and protective finish. Excellent as a general purpose paint. Available in quarts, gallon, 5 gallon pails and drum containers ready for brushing. May be thinned for spray applications. HazMat Charges May Apply for volumes between 1 and 5 Liters UN1263 Packing Group III Hazard Class 3 Features Bake or air dry Meets MIL-E22118; used for coils, armatures and other electrical apparatus Red Alkyd (Brush/Spray/Dip). Used also as a primer, sealer for screws, pipes, vacuum systems and hydraulic fluid chambers. Available in 3 forms: 1201 (general purpose paint), 1201A (Aerosol spray version of 1201), 1201B (Modified 1201).

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  • Specific Gravity, Product 1201
  • Specific Gravity, Product 1201B
  • Solids Content, Product 1201, weight avg.
  • Solids Content, Product 1201B, weight avg.
  • Viscosity, Product 1201
  • Viscosity, Product 1201B
  • Insulation Resistance, Cured, product 1201, @ 90% RH
  • Insulation Resistance, Cured, product 1201A, @ 90% RH
  • Insulation Resistance, Cured, product 1201B, @ 90% RH
  • Dielectric Strength, product 1201, 24 hrs in water, cured
  • Dielectric Strength, product 1201A, 24 hrs in water, cured
  • Dielectric Strength, product 1201B, 24 hrs in water, cured
  • Dielectric Strength, ASTM D115-55, product 1201, dry, cured
  • Dielectric Strength, ASTM D115-55, product 1201A, dry, cured
  • Dielectric Strength, ASTM D115-55, product 1201B, dry, cured
  • Arc Resistance, Cured, product 1201
  • Arc Resistance, Cured, product 1201A
  • Arc Resistance, Cured, product 1201B
  • Flash Point, Product 1201, closed cup
  • Flash Point, Product 1201B, closed cup
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.