MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
SCG Chemicals EL-Lene™ H5814J High Density Polyethylene Injection Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Key Characteristics:
  • Good processability
  • High stiffness
  • High impact strength
  • Balanced properties between shrinkage and warpage
  • Odorless
  • Safe for food contact

Recommended Applications: General purpose injection parts such as utensils, office articles, bottle caps, toy parts

Information provided by SCG Chemicals

Vendors:
Available Properties
  • Specific Gravity, ASTM D1505
  • Environmental Stress Crack Resistance, ASTM D1693, F50, 25% Igepal
  • Linear Mold Shrinkage, Flow, TPE Method
  • Linear Mold Shrinkage, Transverse, TPE Method
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Flexural Modulus, ASTM D790
  • Izod Impact, Notched, ASTM D256
  • Melting Point, ASTM D2117
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
SCG Chemicals Co.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.