MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Bisalloy Steels Wear 450 Thickness 6-20 mm
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Introduction: BISALLOY® WEAR 450 steel may be considered the ‘all-rounder’ of Bisalloy Steels’ wear grades range. With a nominal hardness of 450 HBW but formulated to be readily usable and easily bent, formed, welded, cut and drilled, BISALLOY® WEAR 450 steel is ideal not only for components encountering wear but also structures subject to wear such as tipper truck trailers, rubbish skip bins and concrete agitators.

Applications: On request, Bisalloy Steels can offer impact guarantees for BISALLOY® WEAR 450 steel. Other applications for BISALLOY® WEAR 450 steel include:

  • Drag Line Buckets
  • Dump Truck Wear Liners
  • Liner Plates
  • Chutes
  • Storage Bins
  • Earthmoving Buckets
  • Deflector Plates
  • Ground Engaging Tools
  • Cutting Edges

Key Words: Formerly BisPlate 450
Vendors:
Available Properties
  • Hardness, Brinell
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break, in 50 mm GL
  • Charpy Impact, Longitudinal (10 mm x 10 mm)
  • Boron, B
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As Balance
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.