| Form Tube 420 is high-strength formable precision tube. It has 15% higher elongation values and very narrow tolerances compared with competing products. Available in circular, rectangular, square and special shapes, it comes with different coating and surface options including cold rolled, galvanized, galvannealed and galfan. Customized shapes and other tailoring options are available upon request. Typically uses include light engineering, where formability, uniform quality, different surface options and usability are important. Dimension Range: SSAB Form Tube 420 is available in circular, square and rectangular shapes. Data provided by SSAB. |