MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Covestro Bayblend® FR3050 PC/ABS Blend
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Main characteristics:
• High toughness even at low temperatures
• High dimensional accuracy and stability
• Good paintability
• Good flowability

Grade characteristics:
• Flame-retardant
• Injection molding
• High heat resistant
• Improved chemical resistance and stress cracking behavior

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Moisture Absorption at Equilibrium, ISO 62, 50% RH
  • Water Absorption at Saturation, ISO 62
  • Viscosity, b.o. ISO 11443-A, melt viscosity
  • Linear Mold Shrinkage, Flow, b.o. ISO 2577, 150x105x3mm
  • Linear Mold Shrinkage, Transverse, b.o. ISO 2577, 150x105x3mm
  • Melt Flow, ISO 1133
  • Tensile Strength at Break, ISO 527-1,-2, 50 mm/min
  • Tensile Strength, Yield, ISO 527-1,-2, 50 mm/min
  • Elongation at Break, b.o. ISO 527-1,-2, 50 mm/min
  • Elongation at Yield, ISO 527-1,-2, 50 mm/min
  • Tensile Modulus, ISO 527-1,-2, 1 mm/min
  • Izod Impact, Notched (ISO), ISO 180-A
  • Izod Impact, Notched (ISO), ISO 180-A
  • Izod Impact, Unnotched (ISO), ISO 180-U
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dissipation Factor, IEC 60250
  • Dissipation Factor, IEC 60250
  • Comparative Tracking Index, IEC 60112, Solution A
  • CTE, linear, Parallel to Flow, ISO 11359-1,-2
  • CTE, linear, Transverse to Flow, ISO 11359-1,-2
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75-1,-2
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1,-2
  • Vicat Softening Point, ISO 306, 50°C/h
  • Vicat Softening Point, ISO 306, 120°C/h
  • Flammability, UL94
  • Flammability, UL94
  • Flammability, UL94, UL 94-5V
  • Flammability, UL94, UL 94-5V
  • Melt Temperature, ISO 294, Injection molding
  • Mold Temperature, ISO 294, Injection molding
  • Injection Velocity, ISO 294
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.