MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Elkem (Bluestar Silicones) CAF® 99 AXAD BLACK Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: CAF 99 AXAD BLACK is a two component room temperature vulcanising silicone elastomer.
  • activated acetic,
  • thixiotropic,
  • black.
Applications: CAF 99 AXAD BLACK is mainly used in sealing and bonding applications for :
  • Household electrical appliances: oven fascias, oven door staples, oven door windows, vitroceramic hobs.
  • Glass bonding applications: bonding of boat port-hole glass, cockpit windows.
Advantages: CAF 99 AXAD BLACK cures quickly at room temperature without release of acetic acid and its setting time can be accelerated with temperature. CAF 99 AXAD BLACK sets in confined spaces and in high section thicknesses. CAF 99 AXAD BLACK gives very high mechanical performance levels, very good heat stability, primerless adhesion on many surfaces and good resistance to chemical agents. CAF 99 AXAD BLACK therefore provides perfect assembly and complete sealing when jointing different materials subject to thermal strains.

Information provided by Bluestar Silicones

Vendors:
Available Properties
  • Specific Gravity, ISO R1183, Part A
  • Specific Gravity, ASTM D297, after curing
  • Specific Gravity, ISO R1183, Part B
  • Storage Temperature
  • Hardness, Shore A, ASTM D2240
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Hardness, Shore A
  • Tensile Strength, adhesion on AG 3 aluminum, cure 1 day at RT, 80% cohesive failure
  • Tensile Strength, adhesion on AG 3 aluminum, cure 3 day at RT, 100% cohesive failure
  • Tensile Strength, adhesion on AG 3 aluminum, cure 7 day at RT, 100% cohesive failure
  • Tensile Strength, adhesion on AG 3 aluminum, cure 7 day at RT+3 days at 250°C+1 day at RT, 100% cohesive failure
  • Tensile Strength, ASTM D412
  • Elongation at Break, ASTM D412
  • 100% Modulus, ASTM D412
  • Tear Strength, ASTM D624
  • Compression Set, cured for 7 days, 125°C temp on specimen compressed by 25% for 3 days
  • Compression Set, cured for 7 days, 150°C temp on specimen compressed by 25% for 3 days
  • Compression Set, cured for 1 day, 125°C temp on specimen compressed by 25% for 3 days
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D419
  • Dissipation Factor, ASTM D150
  • Thermal Conductivity, Standard NF x 10021
  • Thermal Conductivity, Standard NF x 10021
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air, Peak
  • Brittleness Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.