| Hostacom TRC 352N NA2 Strm Gry “Preliminary” high melt flow, high flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has excellent impact/stiffness balance, good flowability properties and improved scratch performance. It is typically used for interior automotive applications. Availability: North America Application: Automotive Parts; Instrument Panels; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Good Flow; Good Impact Resistance; Good Stiffness; Scratch Resistant Information provided by LyondellBasell. |