MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Drake Plastics PCTFE Polychlorotrifluoroethylene
Categories: Polymer; Thermoplastic; Fluoropolymer; Polychlorotrifluoroethylene (PCTFE); Molded

Material Notes: Description: DRAKE PCTFE (polychlorotrifluoroethylene) machinable shapes are produced from Arkema’s Voltalef® 302 resin. PCTFE is recognized for its chemical resistance, low flammability and its retention of mechanical properties at cryogenic temperatures.

Typical Applications:

  • Seals & gaskets
  • Diaphragms & impellers
  • Valve seats & pumps
  • Connectors & insulators

Information provided by Drake Plastics.

Vendors:
Available Properties
  • Density, ISO R 1183D, Amorphous
  • Hardness, Rockwell M, ASTM D875
  • Hardness, Rockwell R, ASTM D785
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO R 527
  • Elongation at Break, ISO R 527
  • Elongation at Yield, ISO R 527
  • Flexural Modulus, ISO 178
  • Izod Impact, Notched, ASTM D256 , Type A
  • Volume Resistivity
  • Surface Resistivity per Square
  • Dielectric Strength, IEC 60243-1
  • Melting Point, ISO 3416 C
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 175
  • Flammability, UL94
  • Oxygen Index, Limiting
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.