| IPETHENE® 670 is a low-density polyethylene produced by high-pressure autoclave technology, designed for extrusion coating and lamination. Features: - No additives
- Low neck-in
- Stable web properties
- Good adhesion to substrates
- Good moisture barrier
- Low coating weight
- Good organoleptic properties
Uses: - Coating paper, cardboard, aluminum foil, plastic film and fabric
- Squeezable bottles
- Master-batches
Processing Methods: - Blow molding
- Compounding
- Extrusion coating and lamination
Information provided by Ducor Petrochemicals |