Moplen HP3818 is a homopolymer suitable for injection molding applications. It exhibits a high fluidity combined with a good stiffness. Moplen HP3818 is suitable for food contact. The grade being in development, this is a preliminary datasheet subjected to changes after product industrialization. This grade is not intended for medical and pharmaceutical applications. Status: Developmental Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; Europe Application: Furniture; Housewares Market: Consumer Products Processing Method: Injection Molding Attribute: Good Stiffness; High Flow; Homopolymer Information provided by LyondellBasell. |