MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Polyplastics TOPAS® 9506F-04 COC
Categories: Polymer; Film; Thermoplastic; Cyclo Olefin Polymer

Material Notes: A low glass transition temperature (Tg) extrusion grade for use in food and medical packaging as a discrete layer in multilayer film. It has a low glass transition temperature, and provides excellent clarity, stiffness, water vapor barrier and good thermoformability. TOPAS 9506F-04 is especially recommended for use in blown films due to its higher molecular weight and increased melt strength for better bubble stability.

TOPAS is an amorphous copolymer based on the polymerization of ethylene and nor-bornene using metallocene catalysts. Its property profile can be varied over a wide range by adjusting the chemical structure during polymerization.

Information provided by Polyplastics.

Vendors:
Available Properties
  • Water Vapor Permeability, ISO 15106-3, 90% RH
  • Density, ISO 1183
  • Water Absorption at Saturation, ISO 62
  • Melt Flow, ISO 1133
  • Melt Flow, ISO 1133
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Tensile Modulus, ISO 527-3, Film, MD
  • Tensile Modulus, ISO 527-3, Film, TD
  • Tensile Modulus, ISO 527-2/1A, 1mm/min
  • Elmendorf Tear Strength MD, ISO 6383-2
  • Elmendorf Tear Strength TD, ISO 6383-2
  • Dart Drop Test, ISO 7765-1, F50
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • Glass Transition Temp, Tg, ISO 11357-1,-2,-3, 10°C/min
  • Haze, ISO 14782, film
  • Gloss, ISO 2813, 60° (film)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Polyplastics Co.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.