| Description: TECHNYL® A 218 V25 Natural is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural color. Key Properties: Mechanical performance; Heat stabilized Benefits: The product offers an excellent combination between thermal and mechanical properties. Applications: It is used in a wide variety of industries. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |