  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
EBS ACRAMAXX M10-18 Structural Methacrylate Adhesive
Categories: Polymer; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: ACRAMAXX M10 series structural adhesives are based on methacrylate adhesives and formulated for superior metal bonding performance. The M10 adhesives were developed to withstand post bake oven temperatures up to 380°F (194°C) for up to 30 minutes. The M10 adhesives are available in two working times, M10-6A or M10-18A (Component A). These two adhesive components are formulated to be mixed with a single activator M10-1BNAT (Component B) at a 10:1 mix ratio. These products are designed with fast cure times and high strength to adhere to assemblies of thermoset composites, plastics, and are formulated to be primerless on most metal surfaces.

Bonds to Polyesters, vinyl esters, SMC, epoxies, acrylics, PVC/FPVC/CPVC, polycarbonate, ABS, styrenics, stainless steel, carbon steel, aluminum, coated metals, galvanized metals, and many other composites, thermoplastics, and metals. Does not bond well to polyolefins, TPO, acetal, or fluoropolymers.

Information provided by Engineered Bonding Solutions, LLC (EBS)

Vendors:
Available Properties
  • Density, Component A
  • Density, Component B
  • Viscosity, Component B
  • Viscosity, Component A
  • Tensile Strength, Postcured
  • Elongation at Break, Postcured
  • Modulus of Elasticity, Postcured
  • Adhesive Bond Strength, ASTM D1002, Lap Shear, CRS (lightly sanded), post-cured; Bake 30min @380°F
  • Adhesive Bond Strength, ASTM D1002, Lap Shear, Al (as received), post-cured
  • Adhesive Bond Strength, ASTM D1002, Lap Shear, Al (as received), post-cured; Bake 30min @380°F
  • Adhesive Bond Strength, ASTM D1002, Lap Shear, CRS (lightly sanded), post-cured
  • Adhesive Bond Strength, ASTM D1002, Lap Shear, SS304 (as received), post-cured
  • Adhesive Bond Strength, ASTM D1002, Lap Shear, Galvanneal (as received), post-cured; Bake 30min @380°F
  • Maximum Service Temperature, Air, continuous
  • Maximum Service Temperature, Air, intermittent
  • Minimum Service Temperature, Air, intermittent
  • Minimum Service Temperature, Air, continuous
  • Cure Time, Fixture Time
  • Working Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.