MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Petrothene® NA216000 Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Applications
PETROTHENE NA 216-000 is a general purpose, heavy and medium weight coating resin, capable of coating weights down to 7.0 lbs/ream at line speeds of 1200 ft/min. It can be applied to paper, foil, cellophane, polyester film, and other base stocks by the conventional extrusion coating process. Products made from materials coated with NA 216-000 include flexible packaging milk cartons, set-up cartons and food boards and other materials.

Regulatory Status
NA 216-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply.

Processing Techniques
The maximum recommended melt temperature for NA 216-000 is 625°F.

Physical Properties
These are typical values and not to be construed as specific product limits.

This product is from the former Equistar product line.

Vendors:
Available Properties
  • Density, ASTM D1505
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638, Type IV specimen
  • Elongation at Break, ASTM D638, Type IV specimen
  • Flexural Stiffness, ASTM D790
  • Vicat Softening Point, ASTM D1525
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell LYB (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.