MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
EMS-Grivory Grilon® TSGL-50/4 black 9833 PA666-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 40% Glass Fiber Reinforced

Material Notes: Product description: Grilon TSGL-50/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 50% long glass fibers. Grilon TSGL-50/4 black is characterized by the following key-properties:
  • high stiffness and strength even after conditioning and over a wide temperature range
  • excellent notched impact resistance also at low temperatures
  • low creep
  • high heat distortion temperatures
  • good dimensional stability and little warpage
  • good surface appearance and ease of processing
The product has been designed for injection molding of technical parts especially in the area of die-cast metal replacement. Grilon TSGL-50/4 black is used in the following market segments:
  • automotive
  • mechanical engineering
  • household and appliances
The glass-fibers are aligned in parallel and are just as long as the pellets (usually 10 mm).

Information provided by EMS Grivory.

Vendors:
Available Properties
  • Density, ISO 1183, Dry
  • Water Absorption, Sim. to ISO 62
  • Moisture Absorption, Sim. to ISO 62
  • Linear Mold Shrinkage, Flow, ISO 294-4, 2577
  • Linear Mold Shrinkage, Transverse, ISO 294-4, 2577
  • Ball Indentation Hardness, ISO 2039-1, Conditioned
  • Ball Indentation Hardness, ISO 2039-1, Dry
  • Tensile Strength at Break, ISO 527-1/-2, Conditioned
  • Tensile Strength at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Dry
  • Elongation at Break, ISO 527-1/-2, Conditioned
  • Tensile Modulus, ISO 527-1/-2, Conditioned
  • Tensile Modulus, ISO 527-1/-2, Dry
  • Charpy Impact Unnotched, ISO 179/1eU, Conditioned
  • Charpy Impact Unnotched, ISO 179/1eU, Dry
  • Charpy Impact Unnotched, ISO 179/1eU, Dry
  • Charpy Impact Unnotched, ISO 179/1eU, Conditioned
  • Charpy Impact, Notched, ISO 179/1eA, Dry
  • Charpy Impact, Notched, ISO 179/1eA, Dry
  • Charpy Impact, Notched, ISO 179/1eA, Conditioned
  • Charpy Impact, Notched, ISO 179/1eA, Conditioned
  • Volume Resistivity, IEC 60093, Conditioned
  • Volume Resistivity, IEC 60093, Dry
  • Surface Resistance, IEC 60093
  • Dielectric Strength, IEC 60243-1, Conditioned
  • Dielectric Strength, IEC 60243-1, Dry
  • Comparative Tracking Index, IEC 60112, Conditioned
  • CTE, linear, Parallel to Flow, ISO 11359-1/-2
  • CTE, linear, Transverse to Flow, ISO 11359-1/-2
  • Melting Point, ISO 11357-1/-3, 10°C/min
  • Maximum Service Temperature, Air, ISO 2578, Long Term
  • Maximum Service Temperature, Air, EMS, Short Term
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75-1/-2
  • Deflection Temperature at 8.0 MPa, ISO 75-1/-2
  • Flammability, UL94, IEC 60695-11-10
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
EMS-Grivory (EMS-CHEMIE)

Category Notes
Plastic
PA, Polyamide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.