MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Covestro Bayblock® Base GS Acrylic Basecoat
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Characterization: Bayblock Base GS is a premium 100% acrylic elastomeric basecoat.

Properties / Applications: Bayblock Base GS is a basecoat with excellent adhesion to asphaltic substrates and the ability to help level the profile of existing granulated surfaces. It is a single component, bleed resistant, high build material. Bayblock Base GS has excellent water-resistance and provides long term protection of asphaltic substrates such as Built-up, Modified-Bitumen roofing and composition shingles. Bayblock Base GS bleed resistance helps the suitable reflective topcoat retain its excellent heat reflection properties. This coating works as a breather to prevent moisture build up under the coating. As with any product, use of Bayblock Base GS coating in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Covestro sold their spray polyurethane foam business to Accella in 2017.

Vendors:
Available Properties
  • Density
  • Solids Content, by volume
  • Solids Content, by weight
  • Tensile Strength at Break, ASTM D412, at 20 Mil DFT, after 1000 hours Weatherometer
  • Elongation at Break, ASTM D412, at 20 Mil DFT, after 1000 hours Weatherometer
  • Tear Strength
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Covestro Deutschland AG, Bayer MaterialScience

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.