MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand more corrosive environments than T430 stainless steel. The grade was developed for magnetic applications requiring a very low coercive magnetic field and a very high permeability. IMRE™ is chemically balanced to offer excellent magnetic properties and superior corrosion resistance with excellent machinability and delivers heat to heat consistency. Once an optimum machining setup has been established, machinists can take advantage of increased machining efficiency rates (run “lights-out” production)

Application: Solenoid valves, fuel injectors, irrigation valves and electro-mechanical devices.

Information provided by Schmolz + Bickenbach

Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Cold Drawn Bars
  • Tensile Strength, Cold Drawn Bars
  • Tensile Strength, Yield, Cold Drawn Bars
  • Elongation at Yield, Cold Drawn Bars
  • Reduction of Area, Cold Drawn Bars
  • Electrical Resistivity
  • Magnetic Permeability
  • Magnetic Coercive Force, Hc
  • Magnetic Saturation Flux Density, Bmax
  • Magnetic Remanence, Br
  • Curie Temperature
  • CTE, linear
  • Annealing Temperature, Soft; Air cool
  • Hot-Working Temperature, Flow Stress of 150 MP at 3.6s-1
  • Hot-Working Temperature, Flow Stress of 95 MP at 3.6s-1
  • Hot-Working Temperature, Flow Stress of 60 MP at 3.6s-1
  • Hot-Working Temperature, Flow Stress of 40 MP at 3.6s-1
  • Hot-Working Temperature, Uniformly heating
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.