| Softell TKG 2039N 1 is a 25% glass fiber reinforced PP copolymer. Advanced technologies allowed for a significant properties improvement e.g. very good impact/stiffness balance, excellent scratch resistance, high dimensional stability, high UV-stability, low emissions and very low gloss. The product is available in different color matched, pellet form. This grade is delivered in C12594 color version. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Ductile; Good Dimensional Stability; Good Flow; Haptics; Low Gloss; Low Shrinkage; Low VOC Emission; Low Warpage; Scratch Resistant Information provided by LyondellBasell. |