MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
DuPont Teijin Films Mylar® MO21 Polyester Film, 1000 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Product Description: Mylar® type MO21 films are strong, heavy gauge films that have excellent electrical properties. These films offer exceptional cut-through resistance, low shrinkage, low moisture absorption, and high thermal durability. Mylar® type MO21 films are used as insulation in systems that have been given Class B ratings by Underwriters Laboratories (UL). They also offer product uniformity that enhances processing on automatic slot and wedge insertion equipment.

The inherit mechanical durability of Mylar® type MO21 films and their good dielectric and thermal durability characteristics endow these films with multiple advantages in motors and generators.

Typical Applications: Mylar® type MO21 films are being widely used for electrical insulation in slot liners, wedges and phase insulation for motors and generators. Mylar® type MO21 films are also frequently used in hermetic motor/compressor sealed units, fractional horse power motors, diaphragms, and industrial laminations.

Approvals: UL 94 VTM-2 - for 92-1400 gauge (0.023-0.35mm). UL Recognition - for 92-500 gauge (0.023-0.35 mm) HWI=5, HAI=4, CTI=1; for 700-1400 gauge (0.18-0.35mm) HWI=4, HAI=0, CTI=1

Information provided by DuPont.

Vendors:
Available Properties
  • Density
  • Thickness
  • Film Elongation at Break, MD, ASTM D882A
  • Film Elongation at Break, TD, ASTM D882A
  • Film Tensile Strength at Break, MD, ASTM D882A
  • Film Tensile Strength at Break, TD, ASTM D882A
  • Dielectric Strength, ASTM D149, 1/4" electrode 500 V/sec 25°C in air
  • Dielectric Breakdown, ASTM D149, 1/4" electrode 500 V/sec 25°C in air
  • Comparative Tracking Index
  • Hot Wire Ignition, HWI
  • High Amp Arc Ignition, HAI
  • Specific Heat Capacity, Typical Mylar®
  • Melting Point, Typical Mylar® via DSC
  • Shrinkage, MD, Unrestrained
  • Shrinkage, TD, Unrestrained
  • Refractive Index, typical of Mylar®
  • Optical Density
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
DuPont Teijin Films

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.