MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Microtherm Group Slatted Panel Filament Reinforced Silica Thermal Insulation Panel, Segmented
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material

Material Notes: Microtherm® Slatted Panel is a panel of microporous insulation, covered in woven glass cloth, that is segmented to wrap easily around pipes or circular ducts.
    Properties
  • Opacified blend of filament reinforced silica
  • Clean segmented panels of high temperature insulation
  • Continuous operation at temperatures up to 1000°C (1832°F)
  • Hydrophobic version also available
  • Clean to use and to cut and shape with no health hazards
  • Non combustible
  • Thermal conductivity only 25% (or less) than that of conventional insulation materials at high temperatures
  • Environmentally safe. Contains no respirable fibrers
    Typical applications
  • Petrochemical and power station applications
  • Circular duct sections
  • Hot fuel cells outer casings
  • Fuel cell B.O.P.

Information provided by Microtherm.

Vendors:
Available Properties
  • Density
  • Thickness
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Specific Heat Capacity
  • Thermal Conductivity, @ 245 kg/m³
  • Thermal Conductivity, @ 245 kg/m³
  • Thermal Conductivity, @ 245 kg/m³
  • Thermal Conductivity, @ 245 kg/m³
  • Maximum Service Temperature, Air, for long term exposure
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.