MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Unifrax Fiberfrax® Duraboard® 3000 Ceramic Fiber Board
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.

Duraboard 3000 insulation, the highest temperature rated board manufactured by Unifrax, provides maximum high-temperature stability and shrinkage resistance. Also formulated from a blend of Fiberfrax alumina-silica fibers and Fibermax, Unifrax's patented polycrystalline mullite fibers, Duraboard 3000 insulation derives its exceptional high-temperature capability from an increased Fibermax fiber concentration in the blend. This unique formulation controls shrinkage to a level of only 1.2% after 168 hours at 2700°F / 1482°C.

Description: Formed from a special blend of Fiberfrax alumina-silica fibers and Fibermax® Mullite fibers. These boards give high stability at temperatures up to 2700°F / 1482°C.

Information Provided by Unifrax I LLC

Vendors:
Available Properties
  • Density, Nominal
  • Loss On Ignition
  • Modulus of Rupture, Fired (24 hrs at cont. use)
  • Modulus of Rupture, Green (typ.)
  • Compressive Strength, 5% Deformation; Fired
  • Compressive Strength, 10% Deformation; Fired
  • Compressive Strength, 15% Deformation; Fired
  • Compressive Strength, 5% Deformation; Green
  • Compressive Strength, 10% Deformation; Green
  • Compressive Strength, 15% Deformation; Green
  • Dielectric Strength
  • Melting Point
  • Maximum Service Temperature, Air, Recommended Operating Temperature
  • Shrinkage, at Recommended Operating Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Unifrax I LLC

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.