MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Ametek Pfinodal® P90 Spinodal Copper-Nickel-Tin Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Spinodal hardened alloys are characterized by regular submicroscopic chemical composition fluctuations. These chemical fluctuations occur spontaneously at the aging temperature and their formation is called spinodal decomposition. In the case of Pfinodal, the copper, nickel (15%), and tin (8%) alloying elements are homogeneous throughout the manufacturing process prior to aging. Mill processing requires a solution anneal and quench step to produce a homogeneous single-phase structure. This is followed by cold work and finally a low temperature aging step. The amount of cold work, aging temperature, and time all affect the strength and formability of the final Pfinodal product. AMETEK’s patented powder metallurgy process accomplishes this uniformity, thus ensuring optimum reproducible properties.

Key Features and Benefits

  • Anti-Galling
  • Anti-Seizing
  • Excellent Ductility
  • Excellent Formability
  • Excellent Lubricity
  • Excellent Machinability
  • High Strength and Hardness
  • Non-Corrosive
  • Non-Magnetic
  • Non-Sparking
Applications
  • Bearings
  • Bushings
  • Centralizers
  • Connectors
  • Couplings
  • Drive Train Components
  • Fasteners
  • Motor Components
  • Non-Sparking Tools
  • Pump Shafts
  • Spacers
  • Thrust Washers
  • Well Casing Equipment

Information provided by AMETEK Inc.

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield, 0.2% offset
  • Elongation at Break
  • Modulus of Elasticity, Tension
  • Modulus of Rigidity
  • Charpy Impact
  • Electrical Resistivity, 7.8% IACS
  • Electrical Resistivity, 7.3% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Copper, Cu, Balance
  • Nickel, Ni
  • Other
  • Tin, Sn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.