MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Evonik BREAK-THRU® EM O 7 Surfactants
Categories: Fluid

Material Notes: Product description: Oleic acid polyglycol ester

Application: BREAK-THRU® EM O 7 is a non-ionic, oil-soluble emulsifier for mineral oils, vegetable oils, methyl or ethyl esters of fatty acids, and solvents. It is clear to slightly hazy in mineral oils, methyl or ethyl esters of fatty acids, and fatty oils. BREAK-THRU® EM O 7 is specifically designed for use as an oil in water emulsifier for pesticides. A recommended dose rate is about 1-10 wt. % for mineral oils, and 5-10 wt% for vegetable and methylated vegetable oils.

Properties & Benefits: BREAK-THRU® EM O 7 is an environmentally acceptable emulsifier for mineral and paraffinic oils with reduced foam and can be used as an alternative to Nonyl-phenol Ethoxylate surfactants(NPEs) in a variety of applications. BREAK-THRU® EM O 7 conforms to use as a pesticide inert ingredient pre- and post-harvest under FIFRA 40 CFR 180.910.

Information provided by Evonik

Vendors:
Available Properties
  • Density
  • pH
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Evonik Corporation (Former Evonik Degussa GmbH)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Visit Zeus Inc. for PEEK Tubing
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.