| CPE is one of the most important impact modifiers for the universal plastics market. Compared with other impact modifiers like AIM (Acrylic Impact Modifier), MBS and ABS. Characteristics: The highest chlorine content, lowest molecular weight, excellent flame retardance, excellent flowability, excellent resistance to chemicals and oil. Application: Flame retardant, flexible PVC modification, tapes, coating and foamed products, etc. Information provided by Sundow Polymers Co., Ltd |