MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals Novapol® PF-0118-DP Butene Copolymer LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: PF-0118-DP complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperature or food-type restrictions, subject to technical suitability. It is also biologically and chemically inert.

The NOVA Chemicals Material Safety Data Sheet contains important safety information and should be reviewed before using the product.

Features: Toughness and strength

Additives: Process stabilizer, High slip and antiblock, Process aid

Applications: Trash bags, garment film, bags-on-roll, liners

Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 100-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

Vendors:
Available Properties
  • Density, ASTM D 792
  • Thickness
  • Melt Flow, ASTM D 1238
  • Film Tensile Strength at Yield, MD, ASTM D 882
  • Film Tensile Strength at Yield, TD, ASTM D 882
  • Film Elongation at Break, MD, ASTM D 882
  • Film Elongation at Break, TD, ASTM D 882
  • Elmendorf Tear Strength MD, ASTM D 1922
  • Elmendorf Tear Strength TD, ASTM D 1922
  • Elmendorf Tear Strength, MD, ASTM D 1922
  • Elmendorf Tear Strength, TD, ASTM D 1922
  • Dart Drop, ASTM D 1709/A, F50
  • Dart Drop Test, ASTM D 1709/A, F50
  • Film Tensile Strength at Break, MD, ASTM D 882
  • Film Tensile Strength at Break, TD, ASTM D 882
  • 1% Secant Modulus, MD, ASTM D 882
  • 1% Secant Modulus, TD, ASTM D 882
  • Haze, ASTM D 1003
  • Gloss, ASTM D 2457, 45°
  • Melt Temperature
  • Die Opening
  • Blow-up Ratio (BUR), Optimum
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.