| Softell TKG 317N E C11323 is a 25% glass fiber reinforced PP copolymer, with excellent stiffness, outstanding scratch resistance and high dimensional stability. The product is available indifferent color matched, pellet form. This grade is delivered in C11323 color version. The product reflects the latest advancements in resin synthesis and compounding technology. This product is also available in other colors, new colors can be developed depending on customer requirements. This grade is not intended for medical, pharmaceutical, food and drinking water applications. Availability: Europe Application: Automotive Parts; Interior Automotive Applications; Interior Trims Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; Excellent Stiffness; Good Abrasion Resistance; Good Dimensional Stability; Good Surface Finish; High Toughness; Low Gloss; Low Shrinkage; Low to No Odor; Noise Damping; Pleasing Surface Appearance; Scratch Resistant; Soft; Weldable Information provided by LyondellBasell. |