MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for forged and fabricated parts in aerospace and industrial applications. Its strength is somewhat less that that for Haynes 718 alloy up to about 1400°F (760°C), and lower than that for Haynes R-41 alloy at higher temperatures. Alloy X-750 can be cold-formed in the annealed condition, and may also be hot-formed at temperatures of about 1900°F (1040°C) or above. Weldability is somewhat limited by susceptibility to strain age cracking under conditions of heavy restraint. The alloy exhibits good resistance to oxidizing combustion gas environments at temperatures up to about 1600°F (870°C).

Property data for samples Heat-treated at 1900°F(1040°C) and 1350°F(730°C)/8hr/FC to 1150°F(620°C)/8hr/AC.

Data provided by the manufacturer, Haynes International, Inc.

Vendors:
Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Tensile Strength, Yield
  • Elongation at Break, 2-inch (51 mm) sample
  • Elongation at Break, 2-inch (51 mm) sample
  • Elongation at Break, 2-inch (51 mm) sample
  • Elongation at Break, 2-inch (51 mm) sample
  • Elongation at Break, 2-inch (51 mm) sample
  • Elongation at Break, 2-inch (51 mm) sample
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Rupture Strength, Initial Stress
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Modulus of Elasticity, Dynamic
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Maximum Service Temperature, Air
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Cobalt, Co
  • Iron, Fe
  • Manganese, Mn
  • Nickel, Ni, as balance
  • Niobium, Nb (Columbium, Cb)
  • Silicon, Si
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Haynes International, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.