MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Dow Dow™ 722 LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: DOW LDPE 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist food packaging, sugar pouches, lidding stock and medical packaging. DOW LDPE extrusion coating resins provide optimal neck-in and draw-down performance with minimal taste/odor contribution. DOW Polyethylene 722 is broad molecular weight distribution homopolymer designed to offer good impact strength and crack resistance, with excellent flexibility. The resin has good processability over a wide range of molding conditions.
  • Typical applications include caps/closures
  • Good impact, ESCR with excellent flexibility

Complies with: US FDA 21 CFR 177.1520©2.2; US FDA DMF; EU No 10/2011; Canadian HPFB No Objection (with Limitations). Consult the regulations for complete details.

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: DMF; EU No 10/2011; FDA 21 CFR 177.1520©2.2; Canadian HPFB No Objection

Form: Pellets

Processing Method: Extrusion Blow Molding; Injection Blow Molding

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Vapor Transmission, ASTM F1249
  • ESCR 100% Igepal®, ASTM D1693, F50
  • Melt Flow, ASTM D1238
  • Neck In, 1.0 mil
  • Coating Weight
  • Hardness, Shore D, ASTM D2240, Molded and tested in accordance with ASTM D4976
  • Tensile Strength at Break, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Tensile Strength, Yield, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Elongation at Break, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Elongation at Yield, ASTM D638, Molded and tested in accordance with ASTM D4976
  • Flexural Modulus, ASTM D790B, 2% Secant, Molded and tested in accordance with ASTM D4976
  • Tensile Impact Strength, ASTM D1822, Type S
  • Coefficient of Friction, ASTM D1894
  • Heat Seal Strength Initiation Temperature
  • Melting Point
  • Crystallization Temperature, Peak
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, Unannealed, Molded and tested in accordance with ASTM D4976
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D746, Molded and tested in accordance with ASTM D4976
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.