| Hostacom TRC 1193N C4 C15975 is high melt flow, 1,800 MPa flexural modulus, low density thermoplastic polyolefin (TPO) resin. It has an excellent balance of processability, rigidity, impact, scratch and mar resistance. It is typically used for injection molding of Instrumental Panels and other interior trim parts or components with good surface appearance properties. Availability: Asia-Pacific Application: Instrument Panels; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; Good Moldability; High Flow; High Impact Resistance; High Rigidity; Low Density; Scratch Resistant Information provided by LyondellBasell. |