MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Online Metals
Visit Online Metals for fast service
on small quantity orders.
Pyrotek ISOMAG® 70 Structural Insulation
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C.

Applications

  • Torpedo cars
  • Ladles
  • Tundishes
  • Fume hoods
  • Heat shields
  • Aluminum furnaces
  • Troughs
  • Vacuum degassers

Advantages

  • Low heat losses at higher temperatures
  • Low shrinkage at temperature use limit
  • Highest strength of any high temperature insulating board
  • High temperature rating
  • Asbestos and ceramic fiber free
  • Non wetted by molten aluminum

Information provided by Pyrotek.

Vendors:
Available Properties
  • Density
  • Open Porosity
  • Elongation at Yield, at 6.9 MPA
  • Flexural Strength
  • Compressive Strength
  • Compressive Strength
  • Compressive Strength
  • Thermal Conductivity
  • Thermal Conductivity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous use
  • Maximum Service Temperature, Air
  • Shrinkage, Linear
  • Shrinkage, Thickness
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Pyrotek, Inc.

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.