MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyrolytic Boron Nitride
Categories: Ceramic; Nitride

Material Notes: Anisotropic pyrolytic BN with hexagonal structure, giving enhanced mechanical properties at very high working temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.19 g/ccFired
Porosity 0.00 %Apparent, fully dense
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 23.4 GPa
@Temperature 20.0 °C
Flexural Strength 186 MPa
@Temperature 1200 °C
3-pont
Compressive Strength 373 MPa
@Temperature 1200 °C
Poissons Ratio 0.25"a" direction
Shear Modulus 9.36 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.6
@Frequency 8.00e+9 Hz
"c" direction at 25°C
 5.0
@Frequency 8.00e+9 Hz
"a" direction at 25°C
Dielectric Strength 200 kV/mm
@Temperature 20.0 °C
dc
Dielectric Loss Index <= 0.00090
@Frequency 1.00e+9 - 1.20e+10 Hz,
Temperature 25.0 - 600 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.00 µm/m-°C
@Temperature 20.0 - 250 °C
Thermal Conductivity 1.70 W/m-K
@Temperature 20.0 °C
"c" direction
 104.7 W/m-K
@Temperature 20.0 °C
"a" direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Boron Nitride, Cubic BN, (Borazone)
Boron Nitride, 60% SiO2 - 40% BN
Chesterton 386 Grinding Fluid
99.5% Alumina, thin film substrate
Goodfellow Potassium Aluminosilicate (Muscovite Mica)

CMORG52 / 90430

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.