MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ChevronTexaco 70 Quenching Oil
Categories: Fluid; Quenchant

Material Notes: Features

Chevron Quenching Oil 70 is a premium quality quenching oil.

It is designed to provide controlled cooling of steel which is important in steel hardening. When quenching is started, Chevron Quenching Oil 70 provides a high initial cooling rate inducing maximum hardness, yet once the critical transformation temperature is passed, the ideal fluid cooling rate decreases to eliminate the possibility of stresses and metal distortion.

Applications

Chevron Quenching Oil 70 is recommended for use

  • when deep and uniform hardening is required in steels having small grain size or wide variation in grain size
  • in steels with lean alloy content
  • in parts having variable sections or odd shapes
  • in steels having variable hardenability
This highly stable oil resists the oxidizing effects of quenching and is less sensitive to the effects of agitation. It is highly heat resistant. No additive replacement is required and, in normal service, the product retains the original viscosity indefinitely. Because of its ability to adhere to smooth or shiny surfaces, Chevron Quenching Oil 70 is also recommended for use when parts must retain a bright finish.

Key Words: CPS Number: 233641; MSDS Number: 2582
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 34 °
Viscosity Measurement 113Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 82 SUS
Saybolt Viscosity at 210°F 38 SUS
Kinematic Viscosity at 40°C (104°F) 14.9 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.5 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -15.0 °CASTM D97
Flammability Test 226Fire Point °C
Flash Point 185 °CASTM D92
 
Descriptive Properties
Quenching Time, s10.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hydrogen Chloride, HCl
AISI 1090 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1090 Steel, cold drawn, spheroidized annealed, 19-32 mm (0.75-1.25 in) round
AGC FC 103 PTFE, 15% Glass Fiber
ConocoPhillips Hydroclear® 22 Quench Oil

WCHEV188 / 74803

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.