MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).

Appearance: Translucent spherical pellets

Uses: Injection molding parts

Available in Europe

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.25 g/ccISO 2781
Maximum Moisture Content 0.050
Melt Flow 20 - 35 g/10 min
@Load 8.70 kg,
Temperature 210 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 98ISO 868
Hardness, Shore D 56ISO 868
Tensile Strength, Ultimate 44.0 MPaISO 37
Elongation at Break 610 %ISO 37
Tensile Modulus 0.118 GPaISO 527
50% Modulus 0.0160 GPa
@Strain 50 %
ISO 37
100% Modulus 0.0170 GPa
@Strain 100 %
ISO 37
300% Modulus 0.0250 GPa
@Strain 300 %
ISO 37
Rebound 32 %ISO 4662
Tear Strength 144 kN/mwith incision; ISO 34B
 180 kN/mwithout incision; ISO 34B
Abrasion 48mm3; ISO 4649
Compression Set 24 %
@Temperature 22.0 °C,
Time 252000 sec
ISO 815
 40 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 136 °CA50; ISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 °CInjection
Nozzle Temperature 205 - 215 °CInjection
Zone 1 200 - 210 °CInjection
Zone 2 210 - 220 °CInjection
Zone 3 210 - 220 °CInjection
Zone 4 210 - 220 °CInjection
Drying Temperature 100 °C
Dry Time 2.00 - 3.00 hour
Dew Point -30.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Alliance Polymers Zythane™ 5080A Thermoplastic Polyurethane Elastomer
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Austin Novel Materials Texalan® 598A Polyether-based TPU
Lubrizol Estane® 2102-90A Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade

PNOVEON165 / 55435

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.