MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Saint-Gobain Norton® Tygon® High-Purity  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Tygon® 2275 I.B. helps maintain product integrity during fluid transfer in pharmaceutical and biotechnology applications. Loss of fluid through migration into the tubing or adherence of fluid onto the tubing walls may create inconsistencies in final product results. Tygon® 2275 I.B. is hydrophobic and resists the sorption (absorption/adsorption) of aqueous fluids. This reduction in sorption minimizes the risk of fluid alteration in single or repeat-use applications. Until now, clear, flexible tubing was restricted from use in many applications due to concern of plasticizer extraction. Tygon® 2275 I.B. High Purity Tubing is entirely free of any plasticizers. This unique tubing uses polymer technology to provide a clear (between braid) and flexible tubing choice for sensitive fluid transfer applications.

Features and Benefits:
  • Extremely low sorption to aqueous fluids
  • Plasticizer free
  • Tough braid reinforcement for elevated working pressures
  • Ideal for use with Tygopure™ Sanitary Fittings
  • Meets USP Class VI, FDA and NSF Criteria
Typical applications include Deionized Water Systems, Sterile Fill Lines, Cell Harvest and Media Process Systems, Water for Injection (WFI) Transport, Preservative Fill Lines, Pharmaceutical and Cosmetic Processing, Chemical Transfer.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792-91
Water Absorption <= 0.010 %<= 0.010 %24 hours at 23°C; ASTM D570-95
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 727215 seconds; ASTM D2240-97
Tensile Strength, Yield 13.8 MPa2000 psiASTM D412-97
Elongation at Break 700 %700 %ASTM D412-97
100% Modulus 2.59 MPa
@Strain 100 %
375 psi
@Strain 100 %
ASTM D412-97
Tear Strength 38.6 kN/m220 pliInitial Tear Strength; ASTM D1004-93
Compression Set 84 %
@Temperature 70.0 °C
84 %
@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 187 %187 %ASTM D412-97
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 23.1 kV/mm587 kV/inASTM D149-93
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 51.7 °C125 °F
Brittleness Temperature -77.8 °C-108 °FASTM D746-95
 -70.0 °C-94.0 °FLow Temperature Flexibility; ASTM D380-87
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain Tygon® 2275 High Purity Tubing Formulation
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Saint-Gobain Tygon® LP 1500 Low Permeation Fuel Tubing
Saint-Gobain Tygon® A-60-N Drinking Water Tubing Formulation
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation

PSTGQZ187 / 68701

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.